Skip to content
Seeking US contractor partners IAS AC472 ACCREDITED ★ METAL BUILDINGS ★ AC472 IAS AC472 accreditedIAS AC472
World Steel USA
Welder looking over the stiffeners and end plate of a heavy column

Column stiffeners and end plate under inspection at World Steel, Vietnam.

VT to AWS D1.1

Every weld on your steel, visually inspected and gauged against AWS D1.1

Size, profile, undercut, porosity, craters and cracks, checked by our QC on every weld before a member moves on, in a plant that fabricates 2,500 metric tons of structural steel a month.

The first and widest screen

Every weld is looked at. Here is exactly what the inspector is looking for

Visual testing is the only method applied to every weld on your steel. It is fast, it needs no power or chemicals, and it catches most of the defects that matter before any other test is booked. Done properly it is not a glance: it is a gauged check of size, profile and surface against the AWS D1.1 acceptance criteria, under good light, at the right time, and written down.

If a weld fails visual inspection, no other test is run on it until it is repaired. VT is the gate every other method waits behind.

Quality inspector taking dimensions on a finished steel member Photo
Dimensional check by QC in Vietnam before a member goes on to blasting and paint.

Under the lamp

Six weld profiles, two of them acceptable

Cross-sections of a fillet weld on a T-joint and a groove weld on a butt joint. The shape of the weld face and toes is the first thing the inspector reads.

Acceptable

Flat to slightly convex fillet

Full leg size, smooth blend at both toes.

Fillet welds in depth
Rejectable

Excessive convexity

A sharp notch at the toe concentrates stress.

Fillet welds in depth
Rejectable

Undersized or concave

Throat smaller than the size on the drawing.

Fillet welds in depth
Rejectable

Undercut at the toe

A groove melted into the base metal, measured in depth.

Fillet welds in depth
Acceptable

Groove weld with even reinforcement

Reinforcement within limits, blending into both plates.

Groove welds in depth
Rejectable

Underfill or overlap

Face below the plate surface, or weld metal rolled over the toe.

Groove welds in depth

What the inspector checks

Eight things read on every weld

Each one has an acceptance criterion in AWS D1.1. A weld has to pass all eight before it is released.

Acceptance ruler

Four numbers that show how strict visual acceptance is

0

cracks accepted

Any crack, whatever its size or direction, is rejected.

1 mm

(1/32 in) undercut

Typical limit on material under 25 mm (1 in), statically loaded, with a short allowance for slightly deeper undercut.

0.25 mm

(0.01 in) undercut

Typical limit on cyclically loaded primary members where the weld is transverse to tensile stress.

48 h

wait on Q&T steels

Final visual inspection of welds in quenched and tempered grades such as ASTM A514 waits at least 48 hours, for delayed cracking.

Examples paraphrased from the AWS D1.1 visual acceptance criteria for nontubular connections. Exact limits depend on the edition, the loading and the joint, and the criteria in your specification govern.

The gauge kit

What our QC inspector carries to every weld

Visual testing is a measured check, not an opinion. Each tool answers one question about the weld.

Fillet weld gauges

Leaf gauges read leg size and whether the face is convex or concave.

Multi-purpose weld gauge

Reads reinforcement, undercut depth, throat and bevel angle in one tool.

Hi-lo gauge

Checks alignment and root gap of groove joints before welding.

Temperature indicators

Contact thermometers and temperature crayons for preheat and interpass.

Inspection light

A strong, even light at the weld, with a raking angle for surface detail.

Magnifier and mirror

For craters, toes and welds that cannot be seen straight on.

Camera

Every rejected weld and every closed repair is photographed for the punch list.

Paint marker

Rejected welds are marked on the steel in yellow paint marker, next to the defect.

A valid inspection

Light, distance, a clean surface and the right moment

A visual inspection only counts if the inspector can actually see the weld. These four conditions are set before the gauges come out.

Light

A common reference, ASME Section V Article 9, asks for at least 1,000 lux (100 fc) at the surface.

Distance and angle

The eye within about 600 mm (24 in) of the weld, at no less than 30° to the surface.

Clean surface

Slag and spatter removed, so the inspector sees the weld, not the dirt on it.

The right time

After cooling to ambient, and after the delay the code sets for quenched and tempered steels.

Two welders operating a submerged-arc welding station on a member Photo
Submerged-arc welding of web-to-flange seams in the Vietnam plant.
Fitter comparing a built-up beam with its shop drawing Photo
In the Vietnam shop, fit-up is compared with the shop drawing before final welding starts.
Built-up members with welded stiffeners and drilled clip plates on shop supports Photo
Stiffeners and drilled clip plates welded on, World Steel plant in Vietnam.

Four sets of eyes

How a weld is signed off at our plant

The steps before, during and after welding are laid out on our weld inspection checkpoint page. This is who looks at the finished weld.

Welder

Checks the weld on completion and cleans it, before it leaves the station.

Foreman

Checks weld size and appearance against the shop drawing.

World Steel QC

Inspects and records every weld in the Welding Inspection Report, and marks any reject.

Your third party

Where you designate one, inspects the same welds at hold points in the plant, by video or on arrival.

Who performs it

Who performs VT on your job

The Inspection and Test Plan both sides agree before production names who performs each test, where it happens and how the results come back to you.

In-house, by World Steel QC

Our QC inspects every weld, to written procedures, with calibrated equipment, at the plant in Vietnam.

Or by the third party you designate

Your QA agency, special inspector or testing firm can perform or witness VT at hold points in our plant, live by video alongside our QC, or on arrival at site.

Agreed in the ITP

Each VT line in the Inspection and Test Plan names the method, extent, acceptance criteria and who performs it, before production starts.

Weld types

The welds VT checks on your steel

Each weld type has its own landing: how it is sized, how we weld it, and how it is inspected.

Questions

Visual testing questions from US reviewers

Is every weld visually inspected?

Yes. Every weld is visually inspected by World Steel QC against the AWS D1.1 acceptance criteria and recorded in the Welding Inspection Report. Welders and foremen check first, so most issues are fixed before QC sees them.

Can visual inspection replace UT on full-penetration welds?

No. VT sees only the surface. Where the code or your specification requires UT or RT of a CJP groove weld, VT is done first and the volumetric test follows.

Who can perform VT besides your QC?

The third party you designate, such as your special inspector or a testing agency. It can inspect at hold points in our plant, live by video, or on arrival at site.

Which standard sets the visual acceptance criteria?

AWS D1.1, with separate limits for statically and cyclically loaded connections, unless your specification sets other criteria. Seismic welds follow the added rules of AWS D1.8 where it applies.

What happens to a weld that fails VT?

It is marked on the steel in yellow paint marker, logged with a photo, repaired under a qualified procedure, inspected again and closed with a photo in the punch list.

Do you inspect welds before they are painted?

Yes. Visual inspection and any other NDT are completed and accepted before blasting and coating, so nothing is hidden under the paint.

Send the weld schedule your engineer wants inspected

We show in the ITP how every weld is visually inspected, where your inspector can check them, and how the records reach your data book.