Skip to content
Seeking US contractor partners IAS AC472 ACCREDITED ★ METAL BUILDINGS ★ AC472 IAS AC472 accreditedIAS AC472
World Steel USA

Coatings for footbridges

Coatings built for rivers, roads and salt air

A footbridge is outdoors for decades, often over water. We blast the steel, then apply the system your engineer names: hot-dip galvanizing, an epoxy system of 150 to 200 µm, or zinc under paint. Every reading is recorded before the span is packed.

Cross-section, typical epoxy system

Topcoat50–75 µm
Epoxy build coat100–125 µm
Zinc-rich primer50–75 µm
Blasted steelSa 2½
DFT 150–200 µm total (6 to 8 mils), read on every member

Diagram. Coats and thicknesses follow your engineer’s specification.

Three systems

Zinc, epoxy, or zinc under paint

Each stack is drawn to show what sits on the steel. Your engineer picks the system and the thickness; we apply it and record it.

Hot-dip galvanizing

Members are dipped after fabrication, so zinc covers every face, the inside of box members and the welds.

Best for

Low upkeep, inland and river sites

Epoxy system

Blasted steel, then two or three coats to a total dry film of 150 or 200 µm (6 to 8 mils), as on the Guyana bridges.

Best for

Colour, a smooth finish, most sites

Duplex

A paint system over galvanizing. The zinc protects under any scratch, the paint protects the zinc and gives the colour.

Best for

Coasts, road splash, de-icing salt

Product pages: hot-dip galvanizing, duplex systems and coating quality.

Exposure guide

Where the bridge stands decides the coat

A starting point for the conversation with your engineer, not a specification.

SiteGalvanizingEpoxy systemDuplex
Inland park or campus Best fit Best fit Suitable
River crossing Best fit Best fit Best fit
Over a road with de-icing salt Suitable Suitable Best fit
Coast or salt spray Suitable Suitable Best fit
Feature bridge, colour matters Not the usual choice Best fit Best fit

Bridges by the sea: coastal corrosion protection.

Paint brands

Paint your maintenance crew can buy at home

Coating systems from six brands sold across the US, including their epoxy lines.

  • Jotun
  • PPG
  • Carboline
  • Hempel
  • Nippon
  • International Paint
  • Sold across the US. Maintenance paint is easy to buy near your bridge.
  • UL-certified products. The coating products we use carry UL certification.
  • Trained painters. Our crew is trained and certified by the paint manufacturer.

In our paint hall

Four checks before a member is packed

Surface profile

Blast cleanliness and profile checked before the first coat.

Dry film readings

DFT read on every member and kept with the job record.

Climate log

Humidity and dew point logged so coats cure as the data sheet says.

Photographed

Coated members photographed before they leave the paint hall.

See the hall: blasting and coating at our plant. The standards behind these checks: SSPC blast grades and PA 2 film thickness and AMPP coating inspection.

Splices and touch-up

Clean where bolts clamp, paint in the crate

Slip-critical splices

Contact faces are masked, or coated with a primer qualified for the slip class your engineer sets.

Trial-fitted first

Splices are bolted in our shop, so coated faces meet as they will on site.

Touch-up in the crate

Matching paint and the repair method ship with the span for scratches from transport and the lift.

Site work by others

Bolt tightening and touch-up on site are the scope of the US contractor, our customer.

Paint hall

From the blaster to the finish coat

Crew loading steel parts onto the shot-blasting conveyor
Members in gray finish paint laid out in the paint hall
Looking through the mesh of a galvanized tower ladder cage at its internal bracing
Painted beams with bolted end plates resting on stands below an overhead crane

Questions

Coating a steel footbridge

Which coating is best for a pedestrian bridge over a river?

Hot-dip galvanizing or an epoxy system both work well over fresh water. Pay most attention to the underside and the bottom chord, which stay damp longest, and to drain holes in box members.

What thickness of paint do you apply?

The system your engineer specifies. The Guyana footbridges carry epoxy systems of 150 or 200 µm total dry film thickness (about 6 to 8 mils), applied after blasting, with readings recorded per member.

When should a footbridge use a duplex system?

Where salt reaches the steel: coasts, salt spray and roads that use de-icing salt. Duplex is also a good choice when the owner wants a colour on a galvanized bridge.

Which paint brands do you use?

Coating systems from Jotun, PPG, Carboline, Hempel, Nippon and International Paint, all sold in the US, so maintenance paint is easy to buy.

How are slip-critical splices coated?

The faying surfaces are masked, or given a coating qualified for the slip class shown on the design drawings. Splices are trial-fitted in our shop before shipping.

Need a coating system that suits your site?

Send the location, exposure and the owner’s colour. We propose a system and show the readings we will record.