Skip to content
Seeking US contractor partners IAS AC472 ACCREDITED ★ METAL BUILDINGS ★ AC472 IAS AC472 accreditedIAS AC472
World Steel USA
Built-up members with welded stiffeners and drilled clip plates on shop supports

Stiffeners and drilled clip plates welded on, World Steel plant in Vietnam.

MT of welds and cut edges

Hairline cracks at weld toes and access holes, drawn out by a magnetic field

Yoke MT on fillet welds, weld toes, copes, access holes and repairs, performed in-house or by the third party you designate, in a plant that fabricates 2,500 metric tons of structural steel a month.

Cracks at the surface, and just under it

A magnetic field across the weld, and powder that gathers where a crack breaks it

Steel carries a magnetic field easily. Where a crack cuts across the field, part of it leaks out of the surface, and fine iron particles dusted on the steel collect along the leak. The result is a sharp line, often far wider than the crack itself, that shows a hairline flaw at a fillet toe, an access hole or a repaired weld. It is fast, it works through thin coatings, and it is the method the seismic and crane codes name for these spots.

Magnetize

An electromagnetic yoke placed across the weld sets up a field between its two legs.

Apply particles

Dry powder is dusted on, or a wet suspension is sprayed, while the field is on.

Read the pattern

Particles gather where a crack leaks the field, drawing a line along the flaw.

Judge and record

Relevant indications are measured against the acceptance criteria and written up.

ELECTROMAGNETIC YOKE particles gather field lines in the steel

MT finds what the eye misses at the surface. It does not look deep into a thick weld; that is UT’s job.

The two-direction rule

Two shots on every area, at right angles

A crack is found best when it lies across the field. Two shots at roughly right angles over every area make sure no crack direction is missed.

0°

First shot

The yoke straddles the weld. Cracks running along the weld cut across this field and show.

90°

Second shot

The yoke is turned about 90°. Transverse cracks, invisible in the first shot, now show.

Choosing the particles

Dry, wet visible or wet fluorescent

The written procedure fixes the particle type for each job. The choice trades speed and tolerance for rough surfaces against sensitivity to the finest cracks.

Dry visible powder

Red, gray or yellow

Dusted on a dry surface, read in daylight or shop light. Good on rough welds and hot steel.

Best for: Shop welds, fillet toes, AWS D1.8 seismic welds

Wet visible

Black on white contrast paint

A suspension sprayed over a thin white contrast coat. Finer particles, sharper lines on smoother surfaces.

Best for: Machined or ground surfaces, small indications

Wet fluorescent

Under UV-A light

Glows yellow-green under UV-A light in a darkened area. The most sensitive choice.

Best for: Critical parts, inspection booths, fine cracks

Before the yoke touches your steel

Six equipment and procedure checks

An MT result is only as good as the field behind it. These checks follow ASTM E709 and the written procedure for your job.

Yoke lift test

An AC yoke must lift at least 4.5 kg (10 lb), a DC yoke 18 kg (40 lb), at the pole spacing used.

Field direction and strength

A field indicator, such as a pie gauge or slotted shims, shows the field is strong enough and running the right way.

Bath concentration

For wet particles, the settled volume in a centrifuge tube is checked before work starts.

Light at the surface

White light for visible particles; UV-A intensity and a dark enough booth for fluorescent ones.

Surface temperature

Kept within the range the written procedure and the particle maker allow.

Written procedure

Technique, particles, field checks and acceptance criteria all fixed in a procedure the technician follows.

On a structural steel job

Six places MT is called for, and the code behind each

Fillet weld toes

Toe cracks on stiffeners, clips and flange-to-web fillets.

AIST TR-13 crane girders, your specification

Column k-area

Cracks in the web next to welded continuity plates and doublers.

AISC 341 seismic systems

Copes and access holes

Thermally cut surfaces in heavy flanges and webs.

AISC 360 and AISC 341

Back-gouged roots

The gouged root of a CJP weld, before the back side is welded.

Good practice, your specification

Weld repairs

The excavation before rewelding and the finished repair after.

AWS D1.1 repair rules

Removed tabs and arc strikes

Ground areas where weld tabs, backing or stray arcs were removed.

AWS D1.8 seismic welds

Built-up members with welded stiffeners and drilled clip plates on shop supports Photo
Stiffeners and drilled clip plates welded on, World Steel plant in Vietnam.
Tubular column with a square base plate and bolt holes, crew working behind it Photo
Column with its base plate and anchor-bolt holes, fabricated in the Vietnam plant.
Welded members with drilled end plates laid out side by side Photo
Members with drilled end plates waiting for release, Vietnam plant.

What MT cannot do

Three limits, and the method that covers each

Magnetic steel only

Works on carbon and low-alloy structural steel, not on austenitic stainless steel or aluminum, which need PT.

Near-surface depth

Finds flaws at or just below the surface; it does not reach the middle of a thick groove weld.

Coatings

Thin coatings are allowed only when the procedure shows indications still form through them.

Who performs it

Who performs MT on your job

The Inspection and Test Plan both sides agree before production names who performs each test, where it happens and how the results come back to you.

In-house, by World Steel QC

Our QC performs MT to the extent your specification assigns to the fabricator, to written procedures, with calibrated equipment, at the plant in Vietnam.

Or by the third party you designate

Your QA agency, special inspector or testing firm can perform or witness MT at hold points in our plant, live by video alongside our QC, or on arrival at site.

Agreed in the ITP

Each MT line in the Inspection and Test Plan names the method, extent, acceptance criteria and who performs it, before production starts.

Weld types

The welds MT checks on your steel

Each weld type has its own landing: how it is sized, how we weld it, and how it is inspected.

Questions

Magnetic particle testing questions from US reviewers

When is MT used instead of PT?

On magnetic structural steel MT is usually preferred: it is faster, works on rougher welds and also finds some flaws just below the surface. PT is used on nonmagnetic metals and where a yoke cannot be placed.

Does AWS D1.8 require a particular MT method?

Yes. For the seismic welds it covers, AWS D1.8 Annex G calls for the yoke method with dry visible particles and a written procedure, and rejects any indication shown to be a crack or incomplete fusion, whatever its length.

Who performs the MT on our job?

World Steel QC, to the extent your specification assigns to the fabricator, or the third party you designate. Your agency can test at hold points in our plant or join our QC live by video.

Can MT be done through paint?

Testing is done before blasting and coating. On a coated member, MT through a thin coat is allowed only when the procedure proves indications still form through it.

What acceptance criteria apply?

The AWS D1.1 visual acceptance criteria apply to indications MT reveals, for the loading the weld is designed for, unless your specification sets others. AWS D1.8 rules are added for seismic welds.

Is the steel demagnetized afterwards?

Residual magnetism in structural members rarely matters. Where your specification asks for it, for example ahead of later welding, residual field is checked and removed.

Tell us which welds need MT