Skip to content
Seeking US contractor partners IAS AC472 ACCREDITED ★ METAL BUILDINGS ★ AC472 IAS AC472 accreditedIAS AC472
World Steel USA
Plate checked against its mill certificate at the World Steel material yard

Engineering and codes

Charpy V-notch toughness in structural steel: when to ask and what to write

A grade tells you how strong steel is. It does not tell you how it behaves with a crack in it on a cold day. That is what a Charpy V-notch test measures, and US codes ask for it in specific places. Here is where, and how to order it.

· 7 min read · World Steel USA engineering team

A steel grade promises strength and ductility in a tension test, which pulls a smooth bar slowly at room temperature. Real structures can also see something harsher: a notch or a weld flaw, a sudden load, cold weather and thick material, all at once. Under those conditions some steels fracture in a brittle way, with little energy absorbed. The Charpy V-notch test measures how a steel behaves in exactly that situation. US codes require it in specific places, and project specifications add it in others. This article explains where it applies and how to put it on an order.

The values below are a selection from current editions of AISC 360-22, AISC 341-22 and the ASTM standards named. The editions on the project govern.

What the test measures

A Charpy specimen is a square bar, normally 10 × 10 × 55 mm, with a 2 mm deep V notch machined in the middle. It is cooled or warmed to the test temperature, placed in a pendulum machine and broken with one swing. The energy the specimen absorbs, read from how high the pendulum rises after the break, is reported in joules, often with ft·lbf beside it. Three specimens make a set, and the requirement is usually an average with a lower limit for any single specimen.

Steel tested across a range of temperatures shows a transition: tough and ductile when warm, brittle when cold. The temperature of the requirement is chosen so the steel is on the tough side of that transition at the coldest temperature the member will see in service, with a margin.

Where AISC 360 requires it

AISC 360-22 asks for Charpy testing of heavy material in two cases.

  • Rolled heavy shapes. Section A3.1c applies to hot-rolled shapes with a flange thickness over 50 mm (2 in) that are used as members subject to primary tension from tension or flexure, and that are spliced or connected with complete-joint-penetration groove welds fusing through the thickness of the flange or the flange and web. They must have a minimum average Charpy energy of 27 J (20 ft·lbf) at 21 °C (70 °F), tested at the alternate core location of ASTM A6 Supplementary Requirement S30.
  • Built-up heavy shapes. Section A3.1d applies the same rule to built-up members with plate over 50 mm (2 in) thick in the same conditions, with the plate tested under the A6 supplementary Charpy requirement.

The reason is the combination of thick steel, which cools slowly at the mill and can have lower toughness in its core, and large welds, which add residual stress and possible flaws. The requirement is at room temperature because it is aimed at fabrication and service in enclosed buildings, not cold exposure.

Where AISC 341 requires it

For seismic force-resisting systems, AISC 341-22 Section A3.3 asks for 27 J (20 ft·lbf) at 21 °C (70 °F) in:

  • Hot-rolled shapes with flanges 38 mm (1-1/2 in) thick and thicker.
  • Plate 50 mm (2 in) thick and thicker in built-up members, and in connection plates where inelastic strain is expected under seismic loading.

Seismic welds have their own filler metal toughness rules. AWS D1.8 sets the requirement for demand critical welds, typically 27 J (20 ft·lbf) at −18 °C (0 °F) and 54 J (40 ft·lbf) at 21 °C (70 °F) for buildings in normal temperature service. The AWS D1.8 series covers those rules.

Cold service and exposed structures

Neither AISC rule addresses cold exposure directly. For structures exposed to low temperatures, such as open industrial structures in the northern states, Alaska, pedestrian bridges, cold storage framing below freezing and crane runways in unheated buildings, the engineer sets a Charpy requirement based on the lowest anticipated service temperature. A common approach is to require 27 J (20 ft·lbf) at a temperature at or a set margin below that service temperature.

Bridge steel, under AASHTO and ASTM A709, uses a zone system based on the lowest service temperature and a higher requirement for fracture-critical members. Building engineers sometimes borrow those values for exposed structures. Either way, the temperature and the energy must be written down, because no grade includes them by default, except for a few specifications such as A1085.

Test frequency: H or P

ASTM A673/A673M sets two sampling frequencies for impact tests of structural steel:

  • Frequency H: one set of specimens per heat. The result represents all the material from that heat.
  • Frequency P: one set per plate as rolled, or per piece. Every plate is tested.

Frequency H is common and suits most heavy shapes and plate. Frequency P is chosen for fracture-critical or highly stressed members, where the variation between plates of the same heat matters. It costs more and takes more time, so it is worth deciding early.

Location and orientation

For plate, specimens are normally taken in the longitudinal direction, parallel to the rolling direction, at a stated depth. For heavy shapes, A6 Supplementary Requirement S30 moves the specimen to the alternate core location, near the junction of flange and web, where the steel is slowest to cool and toughness is lowest. AISC 360 calls for S30 for that reason. A test at the normal location of a heavy shape would overstate its toughness at the critical point.

Through-thickness properties

Toughness along the plate is not the same as strength through it. Thick plate loaded across its thickness by large welds on its face, in T and corner joints, box column corners and continuity plates, can suffer lamellar tearing: cracking along planes of inclusions parallel to the surface. Two measures help:

  • ASTM A770/A770M through-thickness tension testing, which reports the reduction of area of a specimen taken across the thickness.
  • Ultrasonic examination of the plate under A6 Supplementary Requirement S8 before welding, to find laminations.

Detailing matters as much as testing: joint design that reduces the through-thickness pull lowers the risk. The engineer decides which measures a job needs.

Writing a Charpy requirement on the order

A complete requirement says:

  1. Which members or plate thicknesses it applies to.
  2. The minimum average energy, and the minimum single value if different, for example 27 J (20 ft·lbf) average.
  3. The test temperature, for example 21 °C (70 °F) or −29 °C (−20 °F).
  4. The supplementary requirement: A6 S5 for plate or S30 for heavy shapes at the alternate core location.
  5. The frequency: H per heat or P per piece, under A673.
  6. The specimen orientation, if not longitudinal.

"Charpy tested steel" alone is not a requirement. Without energy and temperature, a mill cannot test and a reviewer cannot check.

Reading Charpy results on the certificate

The certificate should report, for each set:

  • The three energies and their average.
  • The test temperature.
  • The specimen size, if smaller than full size, because sub-size specimens absorb less energy and requirements are reduced accordingly.
  • The location and orientation.
  • The frequency, H or P.

The mill test certificate article shows where these values sit on a typical certificate.

Weld metal and heat-affected zone

The base metal is only one part of a welded joint's toughness. The weld metal and the heat-affected zone, the band of base metal changed by the heat of welding, have their own toughness. Filler metal toughness is chosen from the electrode classification and, where a project or AWS D1.8 requires it, qualified by testing. Heat input limits in the welding procedure protect the toughness of the heat-affected zone, especially in thick, high-strength plate. A project that asks for Charpy-tested base metal at a low temperature should check that its welding procedures and filler metals reach the same level.

Common mistakes

  • Specifying Charpy for everything. Requiring Charpy on all steel adds cost and lead time without benefit for most members in enclosed buildings. Target the members and thicknesses where the codes or the service conditions call for it.
  • Asking for the wrong location on heavy shapes. A heavy shape tested at the normal flange location instead of the S30 core location may pass where the core would not.
  • Forgetting sub-size specimens. Thin plate cannot yield a full 10 mm specimen. The requirement must allow sub-size specimens with a reduced energy, or the test cannot be done.
  • Mixing up average and single values. A set of three with a good average can still fail if one specimen is below the single minimum.

Charpy and the schedule

Charpy testing is quick in a laboratory, but it adds time to a mill order: specimens are cut, cooled and tested before the plate is released, and frequency P adds a test for every plate. Naming the requirement at bid, rather than at shop drawings, lets the material be ordered once, with the test built in.

How World Steel handles Charpy requirements

World Steel fabricates 2,500 metric tons of structural steel a month in its own IAS AC472-accredited plant in Vietnam, including heavy built-up members, crane girders and seismic frames where notch toughness is routine. The steel comes mainly from leading Vietnamese plate mills, with Japan, Korea, Indonesia and Thailand when a thickness, test temperature or frequency calls for them.

Charpy requirements from your drawings are carried into each mill order, and the steel arrives with EN 10204 3.1 certificates showing the energies, temperature and location. When your inspector wants independent confirmation, check tests run at an ILAC-recognized ISO/IEC 17025 laboratory or at the laboratory you name, and the results are linked to the heat and its piece marks. All our grades are listed on the structural steel materials page. Next in the series: A588 weathering steel.

Quick answers

What is a Charpy V-notch test?

A small bar of steel with a machined V notch is broken by a swinging pendulum at a set temperature. The energy absorbed, in joules (ft·lbf), shows how much the steel resists fast fracture from a notch at that temperature.

When does AISC 360 require Charpy testing?

For rolled shapes with flanges over 50 mm (2 in) and built-up members with plate over 50 mm (2 in), when they carry primary tension and are spliced or connected with complete-joint-penetration groove welds through the thickness. The requirement is 27 J (20 ft·lbf) at 21 °C (70 °F).

Do seismic members need Charpy testing?

AISC 341 asks for 27 J (20 ft·lbf) at 21 °C (70 °F) in heavy shapes with flanges 38 mm (1-1/2 in) and thicker and plate 50 mm (2 in) and thicker in the seismic force-resisting system. Weld filler metal toughness is set separately.

What does test frequency H or P mean?

Under ASTM A673, frequency H means one set of tests per heat and frequency P means one set per plate as rolled or per piece. P costs more and gives more assurance, and is chosen for critical members.

Keep building your steel plan

Go further on USPEB.com

Keep going in the series

ASTM steel grades series

Fifteen in-depth articles on the steel grades a US structural job names: what each ASTM specification covers, its strength and chemistry, where engineers use it, the extra requirements a project can add, and how a grade is sourced, checked and substituted.

Shapes and plate

The grades of the main frame: wide flanges, plate and the carbon steel of connections.

Hollow sections and pipe

Tube columns, braces and pipe, and the wall thickness the design may use.

Extra requirements

The general rules behind every grade, notch toughness and weathering steel.

Bolts, rods and sheet

The grades of what holds the frame together and the cold-formed steel around it.

Sourcing and substitutes

Grades rolled to other standards and how a substitution is asked for.

Bidding a large US project?

Send the bid documents, or just a footprint and an address. Our engineers check them against US code requirements and confirm what World Steel would supply, from a plant that fabricates 2,500 metric tons of structural steel a month.