Skip to content
Seeking US contractor partners IAS AC472 ACCREDITED ★ METAL BUILDINGS ★ AC472 IAS AC472 accreditedIAS AC472
World Steel USA
Shop worker taking a measurement on a steel plate in the yard

Incoming plate is measured at intake, before any cutting, in the Vietnam plant.

Mill test certificates explained

EN 10204 mill test certificates for structural steel, type by type

Every plate, section and coil in a World Steel building arrives with a mill test certificate. This guide explains what EN 10204 types 2.1, 2.2, 3.1 and 3.2 each guarantee, who signs them, how the heat number ties a certificate to your members, and how a US reviewer reads one next to the ASTM grade.

The standard in one paragraph

What EN 10204 is, and what it is not

EN 10204 is the European standard for the inspection documents a manufacturer supplies with metallic products. It defines four document types, what each contains and who validates it. It sets no strength, chemistry or toughness limits: those come from the product specification, which on a US job is the ASTM grade. A mill test certificate, or MTC, is the document; EN 10204 says what kind of document it is.

Last reviewed . A guide for US contractors, engineers and inspectors, written by a fabricator. The standard itself, and the current edition of each ASTM specification, govern. For the steel we buy and the mills it comes from, see US-standard steel materials.

Defines

The type of inspection document: 2.1, 2.2, 3.1 or 3.2, and the basis of inspection behind it.

Names

Who validates each type: the manufacturer, its independent inspector, the purchaser’s inspector or one named by regulation.

Leaves to the grade

Every property limit. ASTM A992, A572 or A36 decides whether the numbers on the certificate pass.

Used worldwide

By mills in Vietnam, Japan, Korea, Europe and beyond. ISO 10474 uses the same four types.

Type 2.1 · 2.2 · 3.1 · 3.2

The four EN 10204 document types, from a promise to a witnessed test

Each step up the ladder adds evidence. Types 2.1 and 2.2 come from the manufacturer alone. Type 3.1 adds results from your own heat, validated by an inspector independent of production. Type 3.2 adds a second inspector from outside the mill.

Non-specific inspection

2.1

Declaration of compliance with the order

Results shown
None. A statement that the products comply with the order.
Validated by
The manufacturer
On a US job
Not enough for structural steel. It names no test result your reviewer can check against an ASTM grade.
Non-specific inspection

2.2

Test report

Results shown
Typical results from the same manufacturing process, not necessarily from the delivered heat.
Validated by
The manufacturer
On a US job
Accepted for some minor items where the specification allows it. Not for primary members, plate or sections.
Specific inspection

3.1

Inspection certificate 3.1

Results shown
Actual chemistry and test results for the heat and test unit delivered.
Validated by
The manufacturer’s authorized inspection representative, independent of the manufacturing department
On a US job
The usual minimum for structural steel from mills outside the US, and what World Steel supplies for every heat.
Specific inspection

3.2

Inspection certificate 3.2

Results shown
Actual results for the delivered product, with the tests witnessed by a second party.
Validated by
The manufacturer’s independent inspector and the purchaser’s authorized inspector, or an inspector designated by official regulations
On a US job
Used when a specification, owner or authority requires witnessed tests. Agreed before the steel is ordered.

The line that matters

Specific or non-specific inspection

The difference between a 2.2 and a 3.1 is not the paper. It is whether the tests were done on the steel you receive.

Non-specific inspection (types 2.1 and 2.2)

Carried out by the manufacturer under its own procedures to show that products made by the same process meet the order. The products tested are not necessarily the ones you receive. The numbers on a 2.2 are typical of the process, not proof for your heat.

Specific inspection (types 3.1 and 3.2)

Carried out before delivery on the products to be supplied, or on test units of which they are part, as the product specification or the order requires. The results on the certificate belong to the steel in your delivery, identified by heat and test unit.

Validation

Who signs each type

A certificate is only as strong as the person who validates it. EN 10204 names that person for each type, and a reviewer should be able to see who it was.

The manufacturer

Validates types 2.1 and 2.2. Any authorized person at the mill may sign; independence from production is not required.

2.1 · 2.2

The mill’s independent inspector

The manufacturer’s authorized inspection representative, independent of the manufacturing department. Validates the 3.1, and co-validates the 3.2.

3.1 · 3.2

The purchaser’s inspector

An inspector authorized by the purchaser, present for the tests at the mill. Co-validates the 3.2.

3.2

An inspector designated by regulation

Where official regulations name the inspector, for example for pressure equipment or some public works, that inspector co-validates the 3.2 instead.

3.2

1991 to 2004

Old type names you still see on specifications

The 2004 edition replaced the 1991 types. Older specifications and some mills still write 3.1.B. Here is what each old type became.

1991 typeWhat it wasSince 2004
2.1Certificate of compliance2.1, renamed declaration of compliance with the order
2.2Test report2.2, unchanged
2.3Specific test reportDropped. Order 3.1 for results on the delivered product
3.1.AInspection certificate, validated by an inspector designated by regulation3.2
3.1.BInspection certificate, validated by the manufacturer’s independent department3.1
3.1.CInspection certificate, validated by the purchaser’s inspector3.2
3.2Inspection report, validated jointly3.2

How to read an MTC

A 3.1 inspection certificate, field by field

An illustrative layout with invented values, following the EN 10168 field codes many mills use. Every certificate looks a little different; the fields that matter are the same. The green pins match the notes beside it.

Illustrative only. All names, numbers and results are invented to show the layout; CE is the IIW carbon equivalent.

What to check in each field

  • Document type

    Says 3.1 (or 3.2) in words, citing EN 10204. A 2.2 or a blank here is not an inspection certificate.

  • Manufacturer

    The mill that made the steel, not a trader. A stockist may add its own cover sheet, but the mill’s document goes with it unchanged.

  • Specification and grade

    The ASTM grade on your drawings, with its edition or type where the specification has types. Dual grades such as A572 Grade 50 / A992 are fine when both are met.

  • Heat number

    The same number is stenciled, stamped or labeled on the steel. This is what ties the certificate to the piece.

  • Product, size and mass

    Matches the plate, section or coil delivered: thickness, profile and quantity on the packing list.

  • Chemistry and carbon equivalent

    Every element inside the grade’s limits. The carbon equivalent matters to the welding procedure.

  • Mechanical and impact results

    Yield, tensile and elongation meet the minimums; Charpy values at the specified temperature where they were ordered.

  • Validation

    Signed or electronically validated by the inspection department, independent of production, with a date.

The five content groups of EN 10168

EN 10168 lists the information an inspection document for steel can carry, in coded groups. Not every mill uses the codes, but most certificates follow the same order.

A

Commercial transaction and parties

Manufacturer, document type and number, purchaser, order and item numbers.

B

Description of the product

Product form, specification and grade, delivery condition, heat or cast number, dimensions, quantity and mass.

C

Inspection and tests

Tensile, hardness and impact results with the test direction, location and temperature, and the chemical analysis.

D

Other tests

Visual and dimensional inspection, ultrasonic testing of plate, or other tests the order asked for.

Z

Validation

Statement of compliance, date, and the name and function of the person validating.

Heat numbers and traceability

Follow one heat number from the ladle to your piece mark

A certificate is evidence only while it stays attached to the steel. The heat number is how it stays attached: on the certificate, on the plate, in our stock, on the cut parts and against each member.

  1. Melt and cast at the mill

    One heat is one melt of steel. The mill samples the ladle for the heat analysis and gives the heat its number.

    Heat analysis
  2. Tests on the test unit

    Tensile and, when ordered, impact samples are taken from the product and tested. Results go on the certificate under the heat number.

    Inspection certificate 3.1
  3. Marked on the steel

    The heat number is stenciled, stamped or labeled on each plate, bundle or coil, so the steel and its certificate can be matched.

    Mill marking
  4. Checked at our gate

    Our incoming inspection matches the marking to the certificate, checks the grade, size and results against the order, and logs the heat.

    Material log by heat
  5. Stored by grade and heat

    Accepted stock is kept by grade and heat number. Steel without a matching certificate is held, not issued.

    Stock record
  6. Cut parts keep the heat

    When plate or sections are cut, the heat number is transferred to the cut parts, so offcuts and remnants stay identified.

    Cutting record
  7. Linked to piece marks

    Each piece mark records the heats used in it. Pick a member on the erection drawing and its certificates open in PEB Studio.

    Material schedule
  8. Handed over with the job

    Certificates and the material schedule go to you in the materials volume of the handover documents.

    Data book

See the gate check on incoming material inspection, the shop side on material intake at our plant, and the member record on digital project control.

EN 10204 and ASTM on one page

How a US project reads an MTC against the ASTM grade

The EN 10204 type tells your reviewer how much to trust the numbers. The ASTM specification tells them whether the numbers pass. Here is what the certificate has to show for the grades we supply most, as minimums from each specification.

ASTM A992

Wide-flange shapes for beams and columns

Yield 345 to 450 MPa (50 to 65 ksi), tensile at least 450 MPa (65 ksi), yield-to-tensile ratio at most 0.85, carbon equivalent at most 0.45 for most shapes.

Both an upper and a lower yield limit: check the yield is not too high as well as not too low.

ASTM A572 Grade 50

Plate, shapes, built-up girder and column plate

Yield at least 345 MPa (50 ksi), tensile at least 450 MPa (65 ksi).

The type (the niobium and vanadium combination) is reported with the chemistry.

ASTM A36

Plates, angles, channels, base plates and fittings

Yield at least 250 MPa (36 ksi), tensile 400 to 550 MPa (58 to 80 ksi).

Often dual-certified with A572 Grade 50 for plate. Use the grade your drawings name.

ASTM A500 Grade C

Cold-formed hollow structural sections

Rectangular and square: yield at least 345 MPa (50 ksi), tensile at least 425 MPa (62 ksi). Round: yield at least 317 MPa (46 ksi).

Round and rectangular sections have different minimums on the same grade.

ASTM A1085

Hollow sections where tighter properties are specified

Yield 345 to 485 MPa (50 to 70 ksi), tensile at least 450 MPa (65 ksi), Charpy V-notch 34 J (25 ft·lbf) at 4 °C (40 °F).

Impact values are part of the grade, so they must be on the certificate.

ASTM A653 and A1011

Coil for cold-formed purlins, girts and deck

Structural steel grade and yield as specified, and for coated A653 sheet the zinc coating designation and mass in g/m² (oz/ft²).

Coil certificates follow ASTM A568 or A924 test reporting; the coil number stands beside the heat number.

Bolts, nuts and washers come with the maker’s test report for their own ASTM specification, traced by lot rather than heat; welding filler metals with the maker’s certificate to their AWS classification. The full list of grades we buy is on ASTM materials.

On a US job

Where the certificates go after they reach the US

Specification and drawings

The Engineer of Record names the ASTM grade for each member and any impact requirement. EN 10204 3.1 is often written in specifications for steel from outside the US, as the document type.

AISC 360 Section A3.1

Test reports made by the manufacturer, or a testing laboratory, to ASTM A6/A6M or A568/A568M and the product specification, are accepted as sufficient evidence that the steel conforms to its ASTM specification. A 3.1 that reports those results serves that purpose.

Submittal review

The US contractor submits the certificates, often with the material schedule, and the Engineer of Record reviews them against the specification. World Steel prepares the package; the approval is the engineer’s.

Special inspection

Where the building code calls for special inspection of structural steel, material identification and the test reports are among the records the inspector verifies. The certificates and heat log are part of the file we supply.

Import record

Steel import declarations ask where the steel was melted and poured. The mill certificate names the mill and heat, which is where that record starts.

Owner’s records

Many owners keep the certificates for the life of the building, for future modifications, insurance and audits.

The melt-and-pour side is explained on Section 232 steel import rules; the special inspection side on IAS AC472 accreditation.

Notch toughness

Charpy V-notch values on the certificate

Toughness is the one property that cannot be read from strength and chemistry. When a job needs it, the impact energy and test temperature appear on the 3.1, and they only appear if they were ordered.

Plate and coil strip racked by grade and heat number in the store Photo
Stock in the Vietnam plant is kept by grade and heat number, so each piece traces to its mill certificate.

Heavy shapes and thick plate

AISC 360 asks for Charpy V-notch testing of hot-rolled shapes with flanges thicker than 50 mm (2 in) and of thick plate when they are spliced or connected with complete-joint-penetration welds in tension: at least 27 J (20 ft·lbf) at 21 °C (70 °F), on samples from the locations the specification sets.

Seismic force-resisting systems

AISC 341 asks for the same 27 J at 21 °C (70 °F) on heavy hot-rolled shapes and thick plate in the seismic force-resisting system. Your Engineer of Record may set stricter values or temperatures in the specification.

Cold service and owner specifications

Steel that will be cold in service, bridges and some industrial owners call for impact tests at lower temperatures. The temperature and energy come from your specification, and they go on the mill order.

Ordered with the steel

Impact tests are run at the mill on samples from the heat. They cannot be added after the steel is rolled, so the requirement is written on the purchase order before production starts.

For the submittal reviewer

Six checks for every mill certificate

  • Document type

    EN 10204 3.1 (or 3.2 where specified) stated in words. Reject a 2.1 or 2.2 offered for plate or sections.

  • Grade and specification

    The ASTM grade, type and, where it matters, edition match the drawings and specification.

  • Product and size

    Thickness, profile and quantity match the steel delivered and the material schedule.

  • Heat number

    Appears on the certificate, on the steel and in the fabricator’s heat log, and links to the piece marks.

  • Results within limits

    Chemistry, carbon equivalent, yield, tensile and elongation inside the grade’s limits; Charpy where required, at the right temperature.

  • Validation

    Signed or electronically validated by the right person for the type, with a date and the mill’s identity.

Warning signs

When a certificate should be questioned

A trader’s letterhead with no mill document

EN 10204 expects an intermediary to pass on the manufacturer’s inspection document without change. A retyped certificate breaks the chain back to the mill.

No heat number, or one that is not on the steel

Without a heat number that also appears on the material, the certificate cannot be tied to anything you received.

Identical results across different heats

Real test results vary from heat to heat. Repeated round numbers suggest typical values, which is a 2.2 in all but name.

Wrong size or product form

A plate certificate for a section, or 12 mm results for 40 mm plate, is not evidence for the steel delivered.

Charpy missing where it was required

If the specification needs impact values and the certificate has none, the steel was not ordered with them. It cannot be fixed on paper.

Edited or unreadable documents

Altered fields, mismatched fonts or a photocopy of a photocopy. Ask for the mill’s original file or verify through the mill.

Inspection certificate 3.2

When a job asks for a 3.2, and how it is set up

Most US structural jobs are well served by 3.1. A 3.2 is for cases where someone outside the mill must witness the tests. It changes the order, the mill schedule and the inspection plan, so it is settled at quote stage, never after the steel is made.

  • An authority or official regulation names an inspector for the material.
  • The owner or Engineer of Record wants their own inspector to witness the mill tests.
  • Critical members where the specification calls for witnessed testing, such as some heavy transfer girders or industrial structures.
  • A project quality plan that lists 3.2 for named products or grades.

Witness points at our own plant are covered on inspector access and in the Inspection and Test Plan.

Inspector walking a line of painted built-up members on the shop floor Photo
Final look at coated members before they are released to packing, World Steel plant in Vietnam.

Our part

The mill certificates World Steel supplies with your steel

We design, fabricate and supply the steel structure from our own plant in Vietnam. Materials come mainly from Vietnamese mills, with mills in Japan, Korea, Indonesia or Thailand when the specification calls for it. The rules below are the same whichever mill rolled the steel.

A 3.1 for every heat

Plate, coil and sections arrive with EN 10204 3.1 certificates from the mill, for each heat, reporting the ASTM grade you specified.

Charpy on request

Where your specification needs notch toughness, the impact test and temperature go on our mill order, and the results come on the 3.1.

Checked before cutting

At our gate each heat is matched to its certificate and checked against the order and the grade. Steel that does not match is held.

Heat to piece mark

Stock is kept by grade and heat, cut parts keep the heat number, and every piece mark records the heats in it.

Open in PEB Studio

Certificates and the material schedule open from your PEB Studio login while the job is still in the shop.

If you need a 3.2

Tell us at quote stage. The mill, the inspector your specification names and the witnessed tests are agreed before the steel is ordered.

Shop worker taking a measurement on a steel plate in the yard Photo
Incoming plate is measured at intake, before any cutting, in the Vietnam plant.
Labeled stacks of steel plate under a gantry crane Photo
Raw plate stock waiting in the World Steel yard, Vietnam.
Quality inspector taking dimensions on a finished steel member Photo
Dimensional check by QC in Vietnam before a member goes on to blasting and paint.

Sources

The standards behind this guide

Reviewed November 20, 2026. The current edition of each standard governs.

Questions from US reviewers

EN 10204 and mill certificate questions we hear most

What is EN 10204?

EN 10204 is the European standard that defines the types of inspection documents a manufacturer supplies with metallic products, such as steel plate, sections and coil. It names four types, 2.1, 2.2, 3.1 and 3.2, and says what each must contain and who must validate it. It does not set any property limits: those come from the product specification, such as an ASTM grade.

What is the difference between EN 10204 2.2 and 3.1?

A 2.2 test report gives results of non-specific inspection: typical values from the same manufacturing process, validated by the manufacturer. A 3.1 inspection certificate gives the actual results of tests on the delivered product or its test unit, validated by the manufacturer’s inspection representative who is independent of production. For structural steel, ask for 3.1.

What is the difference between EN 10204 3.1 and 3.2?

Both report specific inspection of the delivered product. A 3.1 is validated by the mill’s own independent inspector. A 3.2 is validated by that inspector and also by the purchaser’s authorized inspector or an inspector designated by official regulations, who witnesses the tests.

Is a mill test certificate the same as a mill test report?

In practice yes. US mills usually call it a mill test report or certified mill test report, made to ASTM A6/A6M or A568/A568M. Mills in Asia and Europe usually call it a mill test certificate and state the EN 10204 type. What your reviewer checks is the same: grade, heat number, chemistry and test results.

Are EN 10204 3.1 certificates accepted on US projects?

Yes, when they report the results the specified ASTM grade requires. AISC 360 accepts the manufacturer’s test reports made to the ASTM requirements as evidence of conformity, and the Engineer of Record reviews them against the specification. The EN 10204 type describes the document; the ASTM grade sets the numbers.

Can one certificate show both an ASTM grade and EN 10204?

Yes, and that is common. The certificate states the EN 10204 document type, for example 3.1, and reports steel made to an ASTM specification, such as A572 Grade 50 or A992. Some mills also dual-certify to two grades when the steel meets both.

What is a heat number?

The identification of one melt, or heat, of steel. All steel from a heat shares one chemistry. The heat number is printed on the certificate and marked on the steel, and it is the link a fabricator uses to trace each member back to its certificate.

What did 3.1.B mean?

It was a type in the 1991 edition of EN 10204: an inspection certificate validated by the manufacturer’s department independent of production. The 2004 edition replaced it with 3.1. The old 3.1.A, 3.1.C and 3.2 became the new 3.2.

Can a stockist or trader issue a 3.1 certificate?

A distributor can supply a certificate, but under EN 10204 it should pass on the manufacturer’s inspection document without change, and keep the product identifiable so the document still applies. A certificate retyped on a trader’s letterhead, with no mill document behind it, does not trace back to the mill.

Is an electronic or unsigned certificate valid?

EN 10204 allows inspection documents to be issued and validated electronically, provided the validation is identifiable. ASTM test reports printed from an electronic system are also accepted, and the organization issuing them stays responsible for their content even without a handwritten signature.

When are Charpy values needed on a mill certificate?

When the grade itself includes impact testing, as ASTM A1085 does, or when the specification, AISC 360 or AISC 341 calls for notch toughness, typically for heavy shapes, thick plate in welded tension joints, seismic members and steel in cold service. The test has to be ordered with the steel.

What does World Steel supply?

EN 10204 3.1 certificates for each heat of plate, coil and section, reporting the ASTM grade you specify, with Charpy V-notch results on request. Each heat is checked at our gate, kept to the piece marks that use it, and handed over with the material schedule. Where your specification needs 3.2, it is agreed at quote stage.

Does World Steel approve the material for our project?

No. World Steel buys, checks and fabricates the steel and supplies its certificates. Reviewing and accepting the material against the specification is the job of the Engineer of Record and the US contractor, our customer.

See the certificates before the steel is cut

Send drawings or a specification with your grades and any Charpy or 3.2 requirements. We confirm the mills, the certificate type and the material schedule format with the quote.