Skip to content
Seeking US contractor partners IAS AC472 ACCREDITED ★ METAL BUILDINGS ★ AC472 IAS AC472 accreditedIAS AC472
World Steel USA
Rows of roof purlins and rod bracing across a steel frame

Exported steel in place in Thailand: a World Steel job abroad, shown for the building type rather than a US site.

Materials · Sheet and coil

Galvanized, Galvalume and hot-rolled coil, roll-formed into purlins, girts and panels

ASTM A653, A792, A1011 and A755 coil, checked for grade, coating and base metal thickness at our gate, then formed into the secondary frame and envelope in a plant that fabricates 2,500 metric tons a month.

Coil grades

Five ASTM coil products, each slit to the member it becomes

Coil is the raw material of the secondary frame and the building envelope. We roll-form it into purlins, girts and panels in the same plant that fabricates 2,500 metric tons of structural steel a month.

  • ASTM A653

    Hot-dip galvanized (zinc)Regular grade
    Grade
    SS Grade 50 / 55
    Yield
    340 / 380 MPa (50 / 55 ksi)
    Coating
    Z180 – Z275 (G60 – G90)
    Becomes
    Z and C purlins, girts, eave struts and deck
  • ASTM A792

    55% aluminum-zinc (Galvalume)Regular grade
    Grade
    SS Grade 50 / 80
    Yield
    340 / 550 MPa (50 / 80 ksi)
    Coating
    AZ150 – AZ165 (AZ50 – AZ55)
    Becomes
    Roof and wall panels, trims, flashings
  • ASTM A1011

    Hot-rolled sheet and stripRegular grade
    Grade
    SS Grade 50
    Yield
    340 MPa (50 ksi)
    Coating
    Bare, then shop primed
    Becomes
    Heavier purlins and girts, painted after forming
  • ASTM A755

    Prepainted coilRegular grade
    Grade
    On A653 or A792 substrate
    Yield
    Per substrate
    Coating
    Paint system as specified
    Becomes
    Colored roof and wall panels, trims
  • ASTM A1008

    Cold-rolled sheetOn request
    Grade
    SS Grade 40 / 50
    Yield
    275 / 340 MPa (40 / 50 ksi)
    Coating
    Bare
    Becomes
    Light formed parts that are painted or galvanized after forming

Minimum yield values from each ASTM specification for structural steel (SS) grades. "On request" grades are sourced per project and confirmed, with their mill, in your proposal before you order.

Coating weights

Zinc and aluminum-zinc coatings, metric name first

Coating mass is the total of both sides, as a triple-spot test minimum. The G and AZ names come from ASTM A653 and A792 in US units; the Z and AZ metric names are the same coatings in g/m².

  • Z180(G60)

    180 g/m² (0.60 oz/ft²)

    Interior purlins and girts in dry buildings

  • Z275(G90)

    275 g/m² (0.90 oz/ft²)

    The common choice for purlins, girts and exposed framing

  • AZ150(AZ50)

    150 g/m² (0.50 oz/ft²)

    Galvalume roof and wall panels

  • AZ165(AZ55)

    165 g/m² (0.55 oz/ft²)

    Galvalume roofing with the longest panel warranties

Thickness rules

Purlins are designed on the steel, not on the zinc

  • Base metal, not total thickness

    Cold-formed members are designed on base metal thickness, the steel under the coating. A 1.5 mm (0.059 in) purlin is 1.5 mm of steel before zinc.

  • The 95% rule

    AISI S100 accepts delivered steel whose uncoated thickness is at least 95% of the design thickness. We check it with a micrometer at intake, on every coil.

  • Gauge is a habit, not a spec

    US drawings often say “16 gauge”. The order is written in millimetres and inches of base metal, so there is no doubt what was bought.

Read a coil tag

What every coil tag tells your reviewer before it is slit

Every coil that reaches our plant is checked against its tag and its EN 10204 3.1 certificate, then logged in PEB Studio. The purlins formed from it keep that coil number.

Sample coil tag

Specification
ASTM A653/A653MThe standard the coil was made and tested to.
Grade
SS Grade 55 (380)Structural steel grade, minimum yield in ksi and MPa.
Coating
Z275 (G90)Zinc mass on both sides; the inspector checks it against the order.
Thickness
1.90 mm BMTBase metal thickness, the number the purlin is designed on.
Width
1,219 mm (48 in)Slit later to the strip width for each purlin size.
Heat / coil number
Logged at intakeLinks the coil to its 3.1 certificate and to every purlin formed from it.

Questions from US contractors

Steel coil for metal buildings, answered

Which coil grades does World Steel use for purlins and girts?

Usually ASTM A653 Structural Steel Grade 50 or 55 galvanized coil, or ASTM A1011 Structural Steel Grade 50 hot-rolled coil primed after forming, whichever your drawings name. ASTM A1008 cold-rolled sheet is available on request.

What coating weight do you use?

The one in your specification. Z275 (G90) is the common choice for purlins and girts; panels on ASTM A792 Galvalume coil are usually AZ150 (AZ50) or AZ165 (AZ55).

Are your purlins measured by gauge?

No. We design and order by base metal thickness in millimetres with inches beside it, and check each coil at intake against the AISI S100 rule that delivered thickness must be at least 95% of design thickness.

Where does your coil come from?

Mainly from steelmakers and coaters in Vietnam, such as Hoa Phat Group, Formosa Ha Tinh, POSCO, Hoa Sen and Nam Kim. Naming them does not imply a partnership; the mill for each coil is the one on its certificate.

What if the coater certifies to JIS or AS instead of ASTM?

We compare the certified grade, coating mass and mechanical values with the ASTM order and send it to your Engineer of Record. It is used only with written acceptance.

Can I choose the panel color?

Yes. Prepainted coil to ASTM A755 is ordered in the color and paint system your owner selects, from the coater’s range.

A metal building envelope to quote?

Send the drawings and the panel specification. We confirm every coil grade, coating and color and quote the frame, purlins and panels from a plant that turns out 2,500 metric tons a month.