Materials · Grade cross reference
Steel grade cross reference: ASTM grades beside their closest JIS, EN, GB and KS grades
Pick an ASTM grade and see what comes closest in four other systems, with yield metric first and the gaps called out. Comparable is not interchangeable: your Engineer of Record decides, for steel fabricated in a plant that turns out 2,500 metric tons a month.
Raw plate stock waiting in the World Steel yard, Vietnam.
From Vietnam and the region
Many Vietnamese mill products are certified to ASTM, or ASTM and JIS together.
Where a product is dual certified, no comparison is needed. A TCVN-only or JIS-only certificate is compared with the ASTM limits like any foreign grade.
Pick an ASTM grade, see the closest grades in four other systems
The red line on each bar is the ASTM minimum yield. Blue means the comparable grade reaches it; amber means it falls short and would need your engineer to check the design.
Plate and shapes
Hollow sections
Sheet and coil
ASTM A36
250 MPa (36 ksi) minimum yield
Mild carbon steel. Most comparables match on strength; check carbon and toughness if the member is welded heavily.
JIS · Japan
SS400
JIS G 3101
245 MPa (36 ksi)
Lower yield
EN · Europe
S275JR
EN 10025-2
275 MPa (40 ksi)
Comparable strength
GB/T · China
Q235B
GB/T 700
235 MPa (34 ksi)
Lower yield
KS · Korea
SS275
KS D 3503
275 MPa (40 ksi)
Comparable strength
ASTM A572 Grade 50
345 MPa (50 ksi) minimum yield
High-strength low-alloy plate. JIS and KS 490 grades sit slightly lower on yield in their thinnest range.
JIS · Japan
SM490B
JIS G 3106
325 MPa (47 ksi)
Lower yield
EN · Europe
S355J2
EN 10025-2
355 MPa (51 ksi)
Comparable strength
GB/T · China
Q355B
GB/T 1591
355 MPa (51 ksi)
Comparable strength
KS · Korea
SM355B
KS D 3515
355 MPa (51 ksi)
Comparable strength
ASTM A992
345 MPa (50 ksi) minimum yield
W shapes with a maximum yield, a yield-to-tensile ratio of 0.85 or less and a carbon equivalent cap. Only building-structure grades with the same caps come close.
JIS · Japan
SN490B
JIS G 3136
325 MPa (47 ksi)
Lower yield
EN · Europe
S355J2
EN 10025-2
355 MPa (51 ksi)
Comparable strength
GB/T · China
Q345GJB
GB/T 19879
345 MPa (50 ksi)
Comparable strength
KS · Korea
SN355B
KS D 3861
355 MPa (51 ksi)
Comparable strength
ASTM A588
345 MPa (50 ksi) minimum yield
Weathering steel. Comparables are also weathering grades, but the alloy recipe and the atmospheric corrosion index differ.
JIS · Japan
SMA490AW
JIS G 3114
365 MPa (53 ksi)
Comparable strength
EN · Europe
S355J2W
EN 10025-5
355 MPa (51 ksi)
Comparable strength
GB/T · China
Q355NH
GB/T 4171
355 MPa (51 ksi)
Comparable strength
KSNo comparable we list with confidence. Ask us for the specific mill grade.
ASTM A514
690 MPa (100 ksi) minimum yield
Quenched and tempered plate. Toughness class and welding rules must be checked line by line.
JIS · Japan
SHY685
JIS G 3128
685 MPa (99 ksi)
Lower yield
EN · Europe
S690QL
EN 10025-6
690 MPa (100 ksi)
Comparable strength
GB/T · China
Q690D
GB/T 16270
690 MPa (100 ksi)
Comparable strength
KSNo comparable we list with confidence. Ask us for the specific mill grade.
ASTM A500 Grade C
345 MPa (50 ksi) minimum yield
Cold-formed rectangular HSS. the JIS tube grade is lower on yield; EN 10219 S355J2H is the usual comparison.
JIS · Japan
STKR490
JIS G 3466
325 MPa (47 ksi)
Lower yield
EN · Europe
S355J2H
EN 10219-1
355 MPa (51 ksi)
Comparable strength
GB/T · China
Q355B
GB/T 6728
355 MPa (51 ksi)
Comparable strength
KSNo comparable we list with confidence. Ask us for the specific mill grade.
ASTM A53 Grade B
240 MPa (35 ksi) minimum yield
Steel pipe. Comparable pipe grades exist, but sizes follow different schedule systems.
JIS · Japan
STK400
JIS G 3444
235 MPa (34 ksi)
Lower yield
EN · Europe
S235JRH
EN 10219-1
235 MPa (34 ksi)
Lower yield
GB/T · China
Q235B
GB/T 3091
235 MPa (34 ksi)
Lower yield
KSNo comparable we list with confidence. Ask us for the specific mill grade.
ASTM A653 SS Grade 50
340 MPa (50 ksi) minimum yield
Galvanized structural coil. Check coating mass too: Z275 equals G90.
JIS · Japan
SGC490
JIS G 3302
365 MPa (53 ksi)
Comparable strength
EN · Europe
S350GD+Z
EN 10346
350 MPa (51 ksi)
Comparable strength
GB/T · China
S350GD+Z
GB/T 2518
350 MPa (51 ksi)
Comparable strength
KS · Korea
SGC490
KS D 3506
365 MPa (53 ksi)
Comparable strength
ASTM A792 SS Grade 80
550 MPa (80 ksi) minimum yield
High-strength Galvalume panel steel. Elongation is low in every system; check it for formed profiles.
JIS · Japan
SGLC570
JIS G 3321
560 MPa (81 ksi)
Comparable strength
EN · Europe
S550GD+AZ
EN 10346
550 MPa (80 ksi)
Comparable strength
GB/T · China
S550GD+AZ
GB/T 14978
550 MPa (80 ksi)
Comparable strength
KSNo comparable we list with confidence. Ask us for the specific mill grade.
ASTM A1011 SS Grade 50
340 MPa (50 ksi) minimum yield
Hot-rolled structural strip for purlins. Thermomechanical cold-forming grades are the closest match.
JIS · Japan
SS490
JIS G 3101
285 MPa (41 ksi)
Lower yield
EN · Europe
S355MC
EN 10149-2
355 MPa (51 ksi)
Comparable strength
GB/T · China
Q355B
GB/T 1591
355 MPa (51 ksi)
Comparable strength
KS · Korea
SS315
KS D 3503
315 MPa (46 ksi)
Lower yield
Minimum yield for the thinnest thickness range of each standard; most fall as thickness rises. Names and values change between editions, so the certificate and the edition named on it are what count. This chart is a starting point for your engineer, not an approval.
The whole chart
ASTM steel grades and their closest comparables, side by side
Comparable grades share a strength level; they are not interchangeable. Values in amber fall below the ASTM minimum yield.
ASTM steel grades compared with JIS, EN, GB/T and KS grades, minimum yield in MPa
ASTM grade
JIS
EN
GB/T
KS
ASTM A36250 MPa (36 ksi)
SS400JIS G 3101 · 245 MPa
S275JREN 10025-2 · 275 MPa
Q235BGB/T 700 · 235 MPa
SS275KS D 3503 · 275 MPa
ASTM A572 Grade 50345 MPa (50 ksi)
SM490BJIS G 3106 · 325 MPa
S355J2EN 10025-2 · 355 MPa
Q355BGB/T 1591 · 355 MPa
SM355BKS D 3515 · 355 MPa
ASTM A992345 MPa (50 ksi)
SN490BJIS G 3136 · 325 MPa
S355J2EN 10025-2 · 355 MPa
Q345GJBGB/T 19879 · 345 MPa
SN355BKS D 3861 · 355 MPa
ASTM A588345 MPa (50 ksi)
SMA490AWJIS G 3114 · 365 MPa
S355J2WEN 10025-5 · 355 MPa
Q355NHGB/T 4171 · 355 MPa
Ask us
ASTM A514690 MPa (100 ksi)
SHY685JIS G 3128 · 685 MPa
S690QLEN 10025-6 · 690 MPa
Q690DGB/T 16270 · 690 MPa
Ask us
ASTM A500 Grade C345 MPa (50 ksi)
STKR490JIS G 3466 · 325 MPa
S355J2HEN 10219-1 · 355 MPa
Q355BGB/T 6728 · 355 MPa
Ask us
ASTM A53 Grade B240 MPa (35 ksi)
STK400JIS G 3444 · 235 MPa
S235JRHEN 10219-1 · 235 MPa
Q235BGB/T 3091 · 235 MPa
Ask us
ASTM A653 SS Grade 50340 MPa (50 ksi)
SGC490JIS G 3302 · 365 MPa
S350GD+ZEN 10346 · 350 MPa
S350GD+ZGB/T 2518 · 350 MPa
SGC490KS D 3506 · 365 MPa
ASTM A792 SS Grade 80550 MPa (80 ksi)
SGLC570JIS G 3321 · 560 MPa
S550GD+AZEN 10346 · 550 MPa
S550GD+AZGB/T 14978 · 550 MPa
Ask us
ASTM A1011 SS Grade 50340 MPa (50 ksi)
SS490JIS G 3101 · 285 MPa
S355MCEN 10149-2 · 355 MPa
Q355BGB/T 1591 · 355 MPa
SS315KS D 3503 · 315 MPa
What differs
Six things that can differ when the yield matches
This is why a comparable grade goes to your Engineer of Record and is never swapped in on a buyer’s say-so.
Maximum yield and ratio
A992 caps yield at 450 MPa (65 ksi) and the yield-to-tensile ratio at 0.85. Most general grades have no upper limit, which matters for seismic design.
Toughness temperature
JR, J0 and J2 in EN names mean Charpy at 20 °C, 0 °C and −20 °C. A36 and A572 carry no Charpy test unless it is ordered.
Chemistry and weldability
Carbon equivalent and alloy limits differ, and so do preheat needs. Our welding procedures are qualified on the actual base metal.
Section sizes and tolerances
A metric H or tube close to a US size has different properties and tolerances. A size change is a design change, not just a grade change.
Thickness steps
Each standard lowers its minimum yield at different thickness steps. Compare at the plate thickness you are actually using.
Test frequency
Some standards test per heat, some per lot or per plate. The certificate must show what your specification asks for.
Mill certificates
Where the certificates come from, and what we do with them
Our steel comes mainly from mills in Vietnam, with Japan, Korea, Indonesia and Thailand when a specification calls for it. It feeds a plant that fabricates 2,500 metric tons of structural steel a month, so every certificate is checked at our gate.
Dual-certified where possible
Many plate, section and coil products from mills in Vietnam are produced and certified to ASTM, or to ASTM and JIS together. Where that is the case, no comparison is needed.
TCVN certificates
Vietnamese national standards often follow JIS or ISO. A material certified only to TCVN is compared with the ASTM limits in exactly the same way as any other foreign grade.
Japan, Korea, Indonesia, Thailand
When your specification calls for a grade or size not rolled in Vietnam, we source it from those mills, again ordered to the ASTM grade first.
Mills we source from in Vietnam
Hoa Phat Group
Formosa Ha Tinh
POSCO
Hoa Sen
Nam Kim
Naming them does not imply a partnership or endorsement; the mill for each heat is the one on its certificate.
No, it is comparable. SS400 has a lower minimum yield in its thinnest range (245 MPa against 250 MPa) and no carbon limit in some editions. It can be used in place of A36 only if your Engineer of Record accepts it in writing.
Is Q355B equal to A572 Grade 50?+
They are close on minimum yield, 355 MPa against 345 MPa, but chemistry, test frequency and thickness steps differ. Treat it as comparable, not equal, and submit the certificate for acceptance.
Which grade is closest to A992?+
Building-structure grades with a yield cap and yield-ratio limit, such as JIS SN490B, KS SN355B and GB/T 19879 Q345GJB, come closest. General grades like S355J2 match on strength but not on the upper limits that A992 adds.
Who decides whether a comparable grade can be used?+
Your Engineer of Record. World Steel prepares the comparison; the US contractor, our customer, submits it; the EOR accepts or rejects it in writing.
Does World Steel substitute grades without asking?+
Never. Material is ordered to the ASTM grade on your drawings. A comparable grade is only used after written acceptance, and the acceptance stays in the project record.
Why are some comparables marked as lower?+
Because their minimum yield is below the ASTM grade’s. They are not drop-in replacements; your engineer would have to check the design at the lower value.
Do you supply TCVN-certified steel?+
Most structural steel we buy in Vietnam is certified to ASTM, JIS, EN or KS. If a product is certified only to TCVN, we compare it with the ASTM limits and submit it like any other foreign grade.
A mill certificate you need compared?
Send the certificate and your material schedule. Our engineers set it against the ASTM limits for your Engineer of Record, for steel fabricated in a plant that turns out 2,500 metric tons a month.