Weld access holes in seismic frames: geometry, finish and inspection

A weld access hole is a small cut-out in a beam web, and in an earthquake it sits in one of the most stressed spots of the frame. AWS D1.8 sets its shape, its surface finish and how it is inspected. Here is what the shop has to get right.

· 7 min read · World Steel USA engineering team

To weld the bottom flange of a beam to a column with a complete joint penetration (CJP) groove weld, the welder needs room to reach under the beam web. That room is the weld access hole: a cut-out at the end of the web, just above the flange. It also lets the shop insert steel backing and backgouge the root. It looks like a minor detail, but finite element studies cited in the AWS D1.8 commentary show that the stress flow around an access hole is complex and stress levels are very high, even when the hole is made properly. A notch there can start a crack. This article covers what AWS D1.8 Clause 6.11 and Clause 7 require for weld access holes on Demand Critical welds.

Why the shape matters

Clause 3 defines a weld access hole as an opening that permits access for welding, backgouging or inserting backing. The commentary to Clause 1.4.1, item 10, explains why its shape is part of the design: analysis and research have shown the access hole shape can significantly affect how a moment connection behaves. The hole changes how force flows from the beam flange into the web and into the weld. A sharp corner or rough surface concentrates strain, and in an earthquake the steel there may be pushed past yield again and again.

Cracking from access holes was seen occasionally after the Northridge earthquake and was common after the 1995 Great Hanshin (Kobe) earthquake, according to the commentary on Clause 7.6.

Three kinds of geometry

Clause 6.11.1 sets three options for weld access holes on Demand Critical welds:

Geometry When it applies What governs
Standard Default, unless the contract documents say otherwise Dimensions and tolerances of AWS D1.1 or AISC 360
Alternate When the contract documents call for it on beam-to-column moment connections; also allowed at the fabricator's option D1.8 Figure 6.2
Special When the contract documents require a specific shape, including no access hole at all The dimensions and tolerances specified

The commentary adds context:

  • The standard D1.1 shape is acceptable for all SFRS welds, including Demand Critical welds, unless the Engineer specifies otherwise. Some AISC 358 prequalified connections set their own access hole requirements, and nothing in D1.8 overrides those; the Engineer must put them on the contract documents.
  • The alternate shape of Figure 6.2 was developed in the SAC project through finite element analysis and physical testing, and it improved performance for some connections. It has a long, smooth transition from the flange into the web, with a minimum 10 mm (3/8 in) radius at the curved part and controlled surface roughness. It is not needed for every connection, but the fabricator may use it in place of the standard shape at its discretion.
  • A special geometry is for connections whose performance depends on a specific shape, or on having no access hole, such as some end plate connections. Its details and tolerances must be fully defined.

The Engineer is also cautioned not to specify special access holes where they are not justified. Column splices, for example, work fine with the standard shape.

Surface finish: the 13 µm rule

Clause 6.11.2.1 limits surface roughness on access holes to 13 µm (500 µin), using AWS C4.1 sample 4 as a guide for judging thermally cut surfaces. The limit applies to the alternate and special geometries, unless the Engineer specifies otherwise; the standard D1.1 shape follows the D1.1 rules.

The commentary is practical about how to get there:

  • A hole cut freehand with a torch will likely need grinding.
  • A hole cut with a mechanically guided torch may need some cleanup.
  • A hole made by drilling and sawing may need no extra grinding.

The direction of grinding marks that meet the roughness limit does not matter and need not be controlled.

Notches and gouges

Clause 6.11.2.2 deals with notches and gouges in the access hole, including those from thermal cutting and from misaligned saw cuts. They are removed by grinding and faired to a slope of no more than 1:5 against a straight cut surface, or to a radius of at least 10 mm (3/8 in) in the curved part, in a way that keeps the final hole within its required dimensions and tolerances. The depth that can be repaired by grinding is not limited, except by those slope and tolerance limits.

Clause 6.11.2.3 allows deeper notches, ones that grinding cannot fix within the rules, to be repaired by welding under the general repair clause 6.19.2. That means a ground cavity with at least a 6 mm radius, a WPS, preheat of at least 66 °C (150 °F), qualifying electrodes, grinding to a smooth contour within 13 µm, and MT after repair. The commentary adds that the welded area must be ground not only smooth but to sound metal, so no notch, crack or defect remains, and that grinding is the preferred repair. Our article on seismic base metal repair covers Clause 6.19 in detail.

Inspecting the cut surface

Clause 7 adds three inspection rules:

  • Before welding (Clause 7.6). When the QAP requires it, beam copes and weld access holes are inspected for cracks on the cut surface before welding, by magnetic particle testing (MT) or penetrant testing (PT). The commentary notes that AISC 341 calls for this at welded splices and connections when the flange thickness of a rolled shape, or the web thickness of a built-up shape, exceeds 38 mm (1-1/2 in).
  • Repairs in the Protected Zone (Clause 7.7). Any repair to a weld access hole inside a Protected Zone is inspected by MT or PT.
  • MT method (Clause 7.9). MT follows the yoke method and the written procedure rules of Annex G, explained in our article on ultrasonic and magnetic particle testing.

Thick rolled shapes are singled out because heavy sections can have lower toughness in the core and higher residual stress, so a thermally cut edge is more likely to crack.

Copes, the k-area and access holes

Access holes often sit close to the k-area of a rolled shape, the part of the web near the flange that can be cold-worked by rotary straightening at the mill. The D1.8 commentary notes that thermally cut coped beams and weld terminations in the k-area are known sites for cracking in highly restrained joints, and recommends grinding flame-cut surfaces of copes and access holes smooth. Our article on k-area, continuity plate and doubler welding explains the k-area in full.

How access holes are made in the shop

Making a good access hole is mostly a cutting question:

  1. Program the shape. The geometry from the shop drawings, standard, alternate or special, is programmed into the cutting or beam line machine, not drawn by hand.
  2. Cut mechanically. CNC thermal cutting, plasma or laser, or drill-and-saw beam lines give repeatable radii and smooth surfaces.
  3. Check the shape. Templates or gauges confirm the radius, the length along the flange and the height up the web.
  4. Check the finish. Compare the surface against the roughness guide; grind where needed.
  5. Inspect if required. MT or PT of the cut surface before welding where the QAP or AISC 341 calls for it.
  6. Record it. Access hole checks are logged with the piece mark.

Common access hole problems

The same handful of defects turn up on seismic jobs:

  • A sharp corner where the hole meets the flange. The required radius is missing because the cut was finished by hand, leaving a re-entrant corner that concentrates strain.
  • Gouges from a wandering torch. A freehand cut leaves step marks and gouges well beyond the 13 µm limit.
  • A misaligned saw cut. The saw overruns past the drilled radius and leaves a slot-shaped notch in the web.
  • The wrong geometry. The shop uses the standard shape where the contract documents call for the alternate or special shape, or the reverse on a prequalified connection that sets its own limits.
  • Cracks at the cut edge of thick shapes. On heavy flanges and webs, thermal cutting without enough care can leave fine cracks that only MT or PT will find.
  • Weld spatter and arc strikes. Spatter left in the hole, or an arc strike from a stray electrode, creates a small hard spot and a notch.

Each of these is cheap to fix before welding and expensive to fix after, when the hole is next to a finished CJP weld and possibly inside a Protected Zone.

Questions a general contractor can ask

  1. Which access hole geometry applies to each moment connection type, and where is it shown on the shop drawings?
  2. How are access holes cut: CNC, drilled and sawn, or freehand?
  3. How is the surface finish checked, and against what reference?
  4. Does the QAP or AISC 341 require MT or PT of cut surfaces on this project, and when is it done?
  5. How are notches repaired, and how are repairs inside Protected Zones recorded?

How World Steel makes access holes

World Steel uses laser cutting machines that cut steel up to 100 mm thick, for profiles and hole-making, together with automatic beam lines for drilling and sawing. Access hole geometry is taken from the approved shop drawings and programmed, so radii and transitions are repeatable from piece to piece. Cut surfaces are checked for shape and finish at our fit-up checkpoint, and MT or PT before welding is scheduled where the QAP calls for it. Our shop welding procedures and welders are qualified to AWS D1.8, and the checks are recorded in our IAS AC472-accredited quality system.

Learn more about the cutting step on our CNC and laser cutting page.

Quick answers

What weld access hole shape does AWS D1.8 require?

The D1.1 or AISC 360 standard shape unless the contract documents call for the alternate geometry of D1.8 Figure 6.2 or a special geometry. The fabricator may choose the alternate geometry even when it is not required.

How smooth must the access hole be?

For alternate and special geometries, no rougher than 13 µm (500 µin), judged with AWS C4.1 sample 4 as a guide, unless the Engineer says otherwise.

How are notches in an access hole repaired?

By grinding, faired to no steeper than 1:5 on straight cuts or to at least a 10 mm radius in the curved part. Deeper notches may be repaired by welding, then ground smooth and checked by MT or PT.

When are access holes inspected for cracks?

When the QAP requires it, by MT or PT of the cut surface before welding. AISC 341 calls for it at welded splices and connections with rolled-shape flanges or built-up webs over 38 mm thick.

Keep building your steel plan

Go further on USPEB.com

Keep going in the series

AWS D1.8 seismic fabrication series

Twenty in-depth articles that follow a seismic weld from the drawings to the last test report. Each one explains a part of AWS D1.8:2025 in plain terms and lists the checks a general contractor can ask the fabricator about.

Drawings and scope

What the code covers, which welds are Demand Critical, and the data the drawings must carry.

Procedures and welders

The WPS, the restricted access welder test and the bottom flange sequence.

Details and Protected Zones

Access holes, backing, weld tabs, k-area details, Protected Zones and repairs.

Inspection and testing

Who inspects what, inspector qualifications, and UT and MT done the D1.8 way.

Bidding a large US project?

Send the bid documents, or just a footprint and an address. Our engineers check them against US code requirements and confirm what World Steel would supply, from a plant that fabricates 2,500 metric tons of structural steel a month.