Skip to content
Seeking US contractor partners IAS AC472 ACCREDITED ★ METAL BUILDINGS ★ AC472 IAS AC472 accreditedIAS AC472
World Steel USA
Steel frame with beams and metal deck in place on a World Steel office building

Engineering and codes

Protected zone fabrication rules: attachments, erection aids and repairs

A protected zone is the length of steel that is meant to bend and yield in a big earthquake. Anything welded, shot or drilled into it can become the start of a fracture. AWS D1.8 Clause 6.18 sets what is banned there and how mistakes are put right.

· 7 min read · World Steel USA engineering team

A seismic steel frame is designed to survive a large earthquake by letting chosen pieces of steel yield, bend and stretch, absorbing energy while the rest of the frame stays elastic. Those chosen regions are the plastic hinges, and the length of member around each one is the Protected Zone. The steel there must be able to strain far past yield, again and again, without cracking. A shear stud, a clip welded on for a ceiling hanger or a careless tack weld can each leave a notch or a hard spot, and in a yielding beam a notch becomes a crack. AWS D1.8 Clause 6.18, together with the tack weld rules of Clause 6.12, sets the protected zone fabrication rules. This article explains them and how a shop keeps a Protected Zone clean from cutting to shipping.

What a Protected Zone is

Clause 3 defines the Protected Zone as the part of a member of the seismic force-resisting system (SFRS), designated by the Engineer on the contract documents, in which inelastic straining is expected and to which special limits on attachments and fabrication apply. The commentary explains that it is meant to cover the parts of the structure where plastic hinges are expected to form.

Typical examples from the commentary's figures and AISC 341:

  • in moment frames, a length of beam near each beam-to-column connection, for example the reduced section of a reduced beam section (RBS) connection plus some distance beyond
  • in eccentrically braced frames, the link
  • in concentrically braced frames, the brace and its expected buckling regions, and parts of the gusset plates
  • in buckling-restrained braced frames and steel plate shear walls, the regions AISC 341 assigns

D1.8 does not size Protected Zones; AISC 341 and AISC 358 do. Clause 1.4.1 requires the Engineer to show the locations and dimensions of the Protected Zones on the contract documents. The shop drawings then carry them onto each piece. Our landing page on protected zones in seismic frames shows them by system.

What is banned: welded attachments

Clause 6.18.1 is the core rule. Welded attachments are prohibited in the Protected Zone, including stud welds and fasteners for connecting other materials. That covers shear studs, welded clips for cladding, ceiling or pipe hangers, nailers, welded threaded studs and similar items.

The commentary records why. In a moment connection test with a composite floor slab, a fracture started at a welded shear connector in the hinge region. The same researchers found that puddle welds holding metal deck were not a problem, so D1.8 makes one exception: arc spot welds (puddle welds) for attaching metal decking are permitted in the Protected Zone.

AISC 341 adds that power-actuated fasteners up to 4.6 mm (0.18 in) diameter may be used in the Protected Zone, and the D1.8 commentary cites research showing such fasteners had no effect on the cyclic behavior of moment frames.

Erection aids need approval

Erection aids, such as lifting lugs, erection seats, alignment clips and safety cable tabs, are the most common reason someone wants to weld inside a Protected Zone. Clause 6.18.2 says that if erection aids must be attached there, the contractor must obtain the Engineer's approval.

The commentary acknowledges that some aids, including attachments to meet OSHA safety requirements, may be unavoidable. The approval is how the Engineer checks that the attachment will not cause a stress concentration that could fracture in an earthquake. It may also be necessary to remove the aid afterwards and grind the surface to remove any notch effect, and good welding practice, including proper preheat, should be used when aids are attached. In practice, the best approach is to plan erection aids outside Protected Zones from the start, on the shop drawings, so no approval is needed.

Tack welds in the Protected Zone

Clause 6.12 sets three rules that matter most here:

  • Placement (6.12.2). Tack welds outside the weld joint are prohibited in the Protected Zone, unless the Engineer specifically requires or permits them and they are shown on the detail drawings.
  • Backing (6.12.3). Tack welds between steel backing and the beam flange outside the joint are prohibited. Backing tacks go inside the joint where practicable, or to the column for beam flange to column flange welds.
  • Mistakes (6.12.4). Misplaced tack welds are removed by grinding, and gouges and notches are repaired regardless of size, by grinding or by welding at the contractor's choice.

The commentary explains the logic. A tack inside the joint is consumed and tempered by later passes. A tack outside the joint leaves a small hard heat-affected zone and possibly a notch, and it can create an unintended load path. In a zone meant to deform inelastically, neither is acceptable.

Removing welds from the Protected Zone

When a weld in the Protected Zone has to come off, for example a temporary attachment, Clause 6.18.3 sets the method: air carbon arc cutting, grinding, chipping or other thermal cutting, controlled to minimize errant gouging. After removal, the area is ground smooth and must be free of defects.

Clause 6.18.4 covers one specific error: a fillet weld or tack weld placed between steel backing and the beam flange by mistake. The fix:

  1. Remove the weld so it no longer attaches the backing to the beam flange.
  2. Grind the beam flange surface flush, free of defects.
  3. Repair any gouges or notches under Clause 6.18.5.

The commentary explains why this error is singled out. A fillet between backing and column seals the natural unfused plane at the backing edge and reduces stress concentration. A weld between backing and the underside of the beam sends more stress through the backing and magnifies the notch. Our article on weld backing removal and reinforcing fillets covers backing in full.

Repairing gouges and notches

Clause 6.18.5 gives two repair routes:

Route Rule Key limits
Grinding (6.18.5.1) Clause 6.19.1 Ground flush or tapered, no steeper than 1:5 along the member axis and 1:2.5 across it
Welding (6.18.5.2) Clause 6.19.2 Ground cavity of at least 6 mm radius, WPS, preheat at least 66 °C (150 °F), qualifying electrodes, ground to 13 µm, MT after repair

The commentary explains the two slopes. A notch perpendicular to the applied stress is more severe than one parallel to it. Shop drawings rarely show the stress direction, but everyone can see the member axis, so D1.8 assumes stress runs along the axis and demands a gentler taper in that direction. For welded repairs, the commentary notes that repairs are usually made under high restraint, so more preheat is required, and MT confirms there are no surface cracks. The repaired area may be up to 1.5 mm under the original surface, and the slope limits apply to a mound as well as a dip. Our article on seismic base metal repair covers Clause 6.19 in detail.

Mislocated holes, studs, pins and screws

Clause 6.18 closes with three common field and shop errors:

  • Mislocated holes (6.18.6). Where the Engineer requires welded restoration, the contractor develops a procedure that the Engineer approves. Welding follows Clause 6.19.2 and the joint is then ultrasonically tested. The commentary describes one method: fill up to half the depth with temporary steel backing of the same specification, gouge a boat-shaped cavity and weld it with stringer beads, then gouge from the other side to remove the backing completely and finish with stringer beads.
  • Mislocated stud welds (6.18.7). Cut off and ground flush.
  • Mislocated screws and shot pins (6.18.8). Where the Engineer requires a weld repair, the contractor develops a procedure that the Engineer approves; the fastener is removed, the base metal ground and restored under Clause 6.19.2, and the joint is ultrasonically tested.

Clause 7.7 adds that any repair to a weld access hole in the Protected Zone is inspected by MT or penetrant testing (PT).

Most violations happen after the shop

The shop can deliver a perfectly clean Protected Zone, and it can still be ruined on site. The trades that follow the steel erector, such as curtain wall, mechanical, electrical, plumbing and fire protection, often need to hang things from beams, and the beam near the column is a convenient spot. A welded clip for a duct hanger takes minutes to attach and can undo the seismic design.

That is why AISC 341 requires Protected Zones to be clearly identified on the drawings and, in many projects, marked on the steel itself. Marking tells every trade on site where not to weld, drill or shoot, and it makes the special inspector's job easier.

Keeping the Protected Zone clean in the shop

  1. Shop drawings. Show every Protected Zone with its dimensions, taken from the contract documents.
  2. Attachments. Detail all clips, studs and erection aids outside Protected Zones; ask the Engineer where that is not possible.
  3. Tack welds. Tack inside the joint only, and backing to the column, never to the beam flange.
  4. Handling. Use slings and supports that do not gouge the flanges; check for crane and handling damage.
  5. Inspection. Visually check every Protected Zone before painting for arc strikes, tacks, gouges and spatter.
  6. Marking. Mark Protected Zones on the steel where the contract documents or the US contractor require it.

How World Steel handles Protected Zones

World Steel shows every Protected Zone on the shop drawings, keeps clips and erection aids out of them by detailing, and raises an RFI to the Engineer, through the US contractor, when an attachment cannot be moved. In the shop, tack welds in Protected Zones go inside the joint, and the zones are checked for arc strikes, gouges and stray welds before coating. On request we mark Protected Zones on the steel so site trades can see them, and our shop welding procedures and welders are qualified to AWS D1.8. Inspections and any repairs are recorded in our IAS AC472-accredited quality system, and the special inspector can review them remotely through inspector access.

Quick answers

What is not allowed in a protected zone?

Welded attachments, including stud welds and welded fasteners for other materials, are prohibited. Arc spot (puddle) welds that attach metal deck are allowed. Erection aids need the Engineer's approval.

How is a weld removed from a protected zone?

By air carbon arc cutting, grinding, chipping or other thermal cutting, controlled to avoid errant gouging. The area is then ground smooth and must be free of defects.

How are gouges in a protected zone repaired?

By grinding to a taper no steeper than 1:5 along the member axis and 1:2.5 across it, or by welding under Clause 6.19.2 with at least 66 °C preheat, grinding to 13 µm and MT afterwards.

What happens to a mislocated shear stud in a protected zone?

It is cut off and ground flush. Mislocated holes, pins or screws that the Engineer wants weld-restored need a procedure approved by the Engineer, followed by UT.

Keep building your steel plan

Go further on USPEB.com

Keep going in the series

AWS D1.8 seismic fabrication series

Twenty in-depth articles that follow a seismic weld from the drawings to the last test report. Each one explains a part of AWS D1.8:2025 in plain terms and lists the checks a general contractor can ask the fabricator about.

Drawings and scope

What the code covers, which welds are Demand Critical, and the data the drawings must carry.

Procedures and welders

The WPS, the restricted access welder test and the bottom flange sequence.

Details and Protected Zones

Access holes, backing, weld tabs, k-area details, Protected Zones and repairs.

Inspection and testing

Who inspects what, inspector qualifications, and UT and MT done the D1.8 way.

Bidding a large US project?

Send the bid documents, or just a footprint and an address. Our engineers check them against US code requirements and confirm what World Steel would supply, from a plant that fabricates 2,500 metric tons of structural steel a month.