The weak point of an ordinary steel brace is compression. It buckles, bends sideways, loses strength cycle after cycle and eventually fractures at its mid-length hinge. In the 1980s and 1990s, engineers in Japan and then the United States developed a brace that does not do that. The buckling-restrained brace (BRB) yields in tension and in compression, with nearly equal strength both ways, and its force-deformation loops stay full and stable through many cycles. A frame that uses it is a buckling-restrained braced frame (BRBF), covered by AISC 341-22 Section F4, with brace qualification testing in Section K3. This article explains how BRBFs work, how they are designed and what changed in 2022.
How a buckling-restrained brace works
A BRB has two parts that work independently:
- A steel core, typically a flat or cruciform plate of a ductile steel, that carries the full axial force and yields along a reduced section in the middle.
- A restraining casing, usually a steel tube filled with mortar or concrete, or an all-steel assembly, that surrounds the core and prevents it from buckling.
Between them, a slip layer or small gap lets the core slide and expand inside the casing, so the casing does not pick up axial load and does not bind as the core shortens and thickens under compression. Because buckling is restrained, the core can yield in compression just as it yields in tension. The brace's ends, outside the casing, are designed to stay elastic and connect to the frame by bolts, pins or welds.
Why engineers choose BRBF
- Stable hysteresis: full, repeatable loops with no buckling, so energy dissipation is high and predictable.
- Balanced strength: compression strength is only slightly higher than tension strength, so V-type frames do not see the large unbalanced forces of an SCBF.
- Economy: ASCE 7 assigns BRBF a high R of 8, with Ω0 = 2.5 and Cd = 5, so the frame is designed for a low force.
- Tunability: the core area can be sized to the demand at each level, unlike rolled braces that come in fixed steps.
The trade-off is that BRBs are proprietary products, tested by their manufacturers, so the frame design depends on the selected product's properties.
Brace strength: adjusted for reality
A BRB's force grows as it yields and hardens, and its compression force is a little higher than its tension force. AISC 341 accounts for this with two factors obtained from testing:
- ω, the strain hardening adjustment factor, the ratio of the maximum tension force at the design deformation to the yield force.
- β, the compression strength adjustment factor, the ratio of maximum compression force to maximum tension force.
The adjusted brace strengths are then ω Ry Pysc in tension and β ω Ry Pysc in compression, where Pysc is the core's yield force based on its area and specified yield stress. These adjusted strengths drive the capacity design of everything around the brace.
Section F4: frame requirements
Braces
Braces must be qualified by test under Section K3 and used within the limits of that qualification. The core's yield strength is either confirmed by coupon tests or taken from the specified value with Ry, depending on the approach the standard permits.
Beams and columns
Beams and columns in a BRBF are designed for the forces generated when all braces reach their adjusted strengths, in tension and compression. They must meet the moderately ductile width-to-thickness limits of Table D1.1. In V-type and inverted-V configurations, the beam must resist the unbalanced force that arises from the difference between the compression and tension adjusted strengths, which is small compared with an SCBF, and must be braced accordingly. K-type bracing is not permitted.
Connections
Brace connections, including gussets, are designed for the adjusted brace strength in compression, which is the larger of the two, and must not buckle. Gusset stability matters: as the frame drifts, the beam-to-column angle changes, and the gusset at a corner is squeezed and bent by frame action. Designers check the gusset for buckling under the brace force and for the additional demands of frame drift, often adding edge stiffeners or using details that let the beam rotate relative to the column.
Protected zones
The steel core of the brace and the elements that connect the core to the beams and columns are protected zones. Since the casing hides the core, this mostly matters for the brace ends and gussets on site.
Section K3: qualifying the braces
Section K3 sets the cyclic tests that a BRB product must pass:
- A subassemblage test, in which the brace and its end connections are tested in a configuration that imposes the rotations the brace will see in the frame, not only axial deformation.
- A brace test, in which the brace is cycled axially through a defined loading protocol.
The protocol steps the brace through increasing deformations up to twice the deformation corresponding to the design story drift, and the brace must achieve a cumulative inelastic axial deformation of at least a set multiple of its yield deformation, in the order of two hundred times. Test results provide ω and β and confirm that the brace stays stable without fracture or casing failure.
The 2022 change: extrapolation limits
A manufacturer cannot test every brace size it sells. AISC 341 therefore lets test results be applied, or extrapolated, to braces that differ from the tested specimen within limits on core area, yield force, length and details. AISC 341-22 updated those extrapolation limits, giving more flexibility to apply existing test results to a range of brace sizes. For project teams, that means a wider choice of qualified braces without new testing, and for manufacturers, a more practical path to prequalifying a product line.
Where BRBF fits
BRBFs are popular in mid-rise and high-rise buildings in high-seismic regions, especially offices, hospitals, schools and laboratories, where predictable performance and economy matter. They work well in retrofits, because the brace strength can be matched to what an existing structure can take. Data centers and other buildings with sensitive equipment use them for their balanced, stable behavior. See seismic data centers.
BRBF compared with SCBF
| Topic | SCBF | BRBF |
|---|---|---|
| How braces dissipate energy | Tension yielding and compression buckling | Tension and compression yielding, no buckling |
| Hysteresis | Pinched, degrading in compression | Full and stable |
| R factor in ASCE 7 | 6 | 8 |
| Unbalanced load on V-braced beams | Large, after brace buckling | Small, set by β |
| Brace supply | Rolled shapes or HSS from the fabricator | Proprietary products with test data |
| Connection design force | Expected brace strength in tension and compression | Adjusted brace strength, usually compression |
| Post-earthquake | Buckled braces visible and replaced | Core damage hidden inside the casing; evaluation by testing or replacement policy |
Neither system is better in every case. SCBF uses familiar materials and can be fabricated entirely by the steel fabricator; BRBF usually gives lighter frames and more predictable performance, at the cost of a specialist supply chain and closer coordination.
Design tips
- Choose the brace supplier early or specify a performance envelope that several qualified suppliers can meet.
- Check drift and frame action together; gusset damage from frame drift is a known issue.
- Size cores to the demand at each level to avoid an unintentionally strong storey.
- Plan the erection sequence: BRBs are often installed after the frame is plumbed, with bolted connections that accept small adjustments.
Coordination: three parties
A BRBF project involves three parties who must work from the same information:
- The Engineer of Record designs the frame, selects brace capacities and specifies the qualified product or performance requirements.
- The BRB manufacturer supplies braces with qualification test data, ω and β values, core yield strength and connection geometry.
- The steel fabricator designs or details the gussets, beams and columns for the adjusted strengths, fabricates the frame to fit the brace ends and ships the frame and braces to suit the erection sequence.
Getting the manufacturer's data early is essential: gusset sizes, bolt patterns or pin locations and tolerances all depend on it.
Fabrication notes
- Gussets for BRB connections are often large and thick; they are cut to the manufacturer's bolt or pin pattern and to the clearances needed for frame drift.
- Tolerances on work points and gusset positions are tight, because BRBs have limited length adjustment.
- Welds joining gussets to beams and columns are designed for the adjusted compression strength.
- Protected zones at brace connections are kept clear of attachments.
How World Steel works on buckling-restrained braced frames
World Steel designs and fabricates the steel frames for BRBF projects in the US, including beams, columns, gusset plates and bracing connections, in its own IAS AC472-accredited plant in Vietnam. We work from the BRB manufacturer's qualification data and connection geometry selected by the Engineer of Record, design or detail gussets and frame members for the adjusted brace strengths, check gusset stability under frame action and hold the tight work-point tolerances BRBs require. Gussets are cut on laser machines that handle steel up to 100 mm thick, and welders are qualified to AWS D1.8.
Our shop drawings show the brace work points, connection geometry and protected zones, and every frame member is tracked in PEB Studio. The Engineer of Record reviews and approves the design; the braces themselves come from the qualified manufacturer, and the US contractor installs them with the frame on site.
The next article covers the last steel system in Chapter F: steel plate shear walls.
Quick answers
How does a buckling-restrained brace work?
A steel core carries the axial force and yields in tension and compression. A casing, usually a steel tube filled with mortar or an all-steel assembly, stops the core from buckling, with a slip layer so the casing carries no axial load.
How are buckling-restrained braces qualified?
By cyclic tests under AISC 341 Section K3: a subassemblage test that includes the brace end rotation and a brace test, loaded to deformations of twice the design story drift deformation, with a minimum cumulative inelastic deformation.
What changed for BRBF in AISC 341-22?
The 2022 edition updated the limits on how far test results may be extrapolated to braces of different sizes and details, giving brace manufacturers more flexibility to prequalify their products.
Who supplies the braces?
Buckling-restrained braces are usually proprietary products supplied by specialist manufacturers with test data. The steel fabricator supplies the frame, gussets and connections designed for the braces adjusted strengths.
Keep building your steel plan
Go further on USPEB.com
On this topic
Across the US market
- US codes and standardsIBC, AISC, AWS and MBMA, designed to
- Seismic steel structuresSDC D to F framing for West Coast jobs
- Crane building designUS crane standards for mill and bay buildings
- Design ReportWhat our US-code design report contains
- Large projects, 2,500 t a monthCapacity for large US general contractors
- Contractor partnershipLong-term supply for US contractors